Home        Products       Services       Locate a Distributor     Repair Products & Info     Custom Colors

SURFACE SPALLING OR DETERIORATION

Surface Spalling 
or Delamination

Basic Preparation

Advanced Preparation

 
             Prepared Area                                         Filled Area                   

REPAIR PROCEDURES
1.Make two cuts at outer edges of spalling, 1/2" deep min.

After cuts are made, deepen the defect to the depth shown with a bush hammer or other means.
Remove all dust and loose concrete.

 

2. Mix Armor-Hard or MM-80 epoxy. Add aggregate to liquid epoxy. Mix per instructions and apply. Compact mortar with trowel from kit to ensure full contact. Trowel smooth or broom finish during epoxy cure non-skid texture.

OPTION: Spal-Pro 2000 Polyurea Repair Polymer can be used if access time is critical.